Chromium-free silicon iron anode
Composition :
Silicon: 14.25 – 15.25%
Manganese: 1.00% max.
Carbon: 1.00% max.
Phosphorus: 0.25% max.
Sulphide: 0.10% max.
Chromium: -
Iron: balance
Cable: HO7RNF1x16mm² (5 meters) or PC 1x10mm² (5 meters)
In sea water
Consumption: 0.50 kg/amp/year
Density: 10-50 Amp / m²
In fresh water
Consumption: 0.15 kg/amp/year
Density: 10-30 Amp / m²
With Backfill coating
Consumption: 0.10 kg/amp/year
Density: 15-50 Amp / m²
The head of the Iron Silicon anode can be reinforced mechanically to avoid any risk of separation.